Airdry can be used like a standard pottery body but it has not to be fired in a ceramic kiln. Drying on air or even better in the kitchen oven gives enough hardness.
Is suitable for modelling, for fitting,
moulding, cutting
and stamping.
After shaping you should dry 24 h at room temperature and after it will be best (but not necessary) 2 h in the kitchen oven at 110° C.
Available in the colours white (no. 191) and red ( no. 391).
After it could be decorated with acrylic colours.
The product could be cleaned with a moist cloth but it's not water resistant.